Highlights of Investment Casting Zone at The 24th China International Foundry Expo

Over 130 investment casting enterprises showcased silica sol casting, 3D printed wax patterns and intelligent production lines at the 24th China International Foundry Expo. The industry shifts toward aerospace, medical and new energy high-end castings, stepping into micron-level precision manufacturing with simulation technology cutting product defects greatly.

Read More